Material Notes:
Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information provided by Ter Hell Plastic GMBH.
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ISO 1183
Water Absorption 8.0 %
8.0 %
ISO 62
Moisture Absorption at Equilibrium 2.1 %
2.1 %
ISO 62
Mechanical Properties Metric English Comments
Tensile Strength 65.0 MPa
9430 psi
dry; ISO 527
Tensile Strength, Yield 70.0 MPa
10200 psi
dry; ISO 527
Elongation at Break 20 %
20 %
dry; ISO 527
Elongation at Yield 2.5 %
2.5 %
dry; ISO 527
Tensile Modulus 2.90 GPa
421 ksi
dry; ISO 527
Charpy Impact Unnotched NB
NB
dry; ISO 179
Charpy Impact, Notched 0.900 J/cm²
4.28 ft-lb/in²
dry; ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ISO 75
Vicat Softening Point 196 °C
385 °F
B 120; ISO 306
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
Electrical Properties Metric English Comments
Comparative Tracking Index 550 V
550 V
IEC 60112
Processing Properties Metric English Comments
Processing Temperature 240 - 270 °C
464 - 518 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour