Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 41.1 °C | 106 °F | ASTM D1525 |
M. Holland Company MAGMA® Magmalene Polyalphaolefin
(discontinued **) High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessUses: BlendingProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Vicat Softening Point | 41.1 °C | 106 °F | ASTM D1525 |
M. Holland Company MAGMA® LM372-A LLDPE
(discontinued **) Features: High Clarity, Good Flexibility, Good Flow, High Gloss, Good ToughnessProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Vicat Softening Point | 41.0 °C | 106 °F | ISO 306 |
Total Evatane® 28 - 05 HDPE vinyl acetate copolymer, blown film, injection molding
(discontinued **) EVA Copolymer made by high pressure tubular process. Temperature profile (°C) for injection molding: 120 to 150.Information provided provided by Total Petrochemicals.Total Petrochemicals includes f.. |
|||
Vicat Softening Point | 41.1 °C | 106 °F | ASTM D1525 |
ExxonMobil Escorene® UL 7620 Adhesive Application Resin
(discontinued **) Escorene Ultra UL 7620 is a medium flow rate, 24% vinyl acetate copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt adhesives, s.. |
|||
Vicat Softening Point | 41.0 - 133 °C | 106 - 271 °F | Average value: 117 °C Grade Count:51 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Vicat Softening Point | 41.0 °C | 106 °F | |
Dow AFFINITY™ SM 8400 Polyolefin Elastomer Data provided by Dow Chemical. |
|||
Vicat Softening Point | 41.0 °C | 106 °F | ASTM D1525 |
Dow Engage® 8400 Polyolefin Elastomer Description: Engage® 8400 and Engage® 8407 polyolefin elastomers are ethylene-octene copolymers that offer excellent performance in durable injection molded industrial and consumer goods and compr.. |
|||
Vicat Softening Point | 41.0 °C | 106 °F | ASTM D1525 |
Dow Engage® 8407 Polyolefin Elastomer Description: Engage® 8407 polyolefin elastomer is an ethyleneoctene copolymer with a nominal loose talc coating. The talc is untreated and has a 1µm particle size. Engage® 8407 offers excellent p.. |
|||
Vicat Softening Point | 41.0 °C @Load 1.02 kg |
106 °F @Load 2.25 lb |
ASTM D1525 |
Arkema Group LOTRYL® 30 BA 02 Copolymer Ethylene - Butyl Acrylate LOTRYL® 30 BA 02 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 30 BA 02 is used for polymer modification, in compounds formula.. |
|||
Vicat Softening Point | 41.0 °C @Load 0.999 kg |
106 °F @Load 2.20 lb |
ISO 306 |
Arkema Group EVATANE® 18-150 Copolymer Ethylene - Vinyl Acetate EVATANE® 18-150 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 18-150 is stabilized with antioxidants. The High Vinyl Acetate .. |
|||
Vicat Softening Point | 41.0 °C @Load 0.999 kg |
106 °F @Load 2.20 lb |
ISO 306 |
Arkema Group EVATANE® 28-03 Copolymer Ethylene - Vinyl Acetate EVATANE® 28-03 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 28-03 is stabilized with antioxidants. The High Vinyl Acetate co.. |
|||
Vicat Softening Point | 41.1 - 130 °C | 106 - 266 °F | Average value: 96.1 °C Grade Count:62 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Injection Molded". Each property range of values reported is mi.. |
|||
Vicat Softening Point | 41.0 °C | 106 °F | B (50N); ISO 306 |
Borealis Daplen™ ED135AI TPO Compound Daplen ED135AI is a 10% mineral filled grade intended for injection molding. ED135AI offers very good balance in stiffness/impact strengthDaplen ED135AI has been developed especially for the car in.. |