Thermal Properties Metric English Comments
Vicat Softening Point 42.0 - 123 °C
108 - 253 °F
Average value: 93.7 °C Grade Count:101
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant". Each property range of values rep..
Vicat Softening Point 65.0 - 123 °C
149 - 253 °F
Average value: 101 °C Grade Count:63
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum ..
Vicat Softening Point 111 - 123 °C
232 - 253 °F
Average value: 117 °C Grade Count:12
Overview of materials for Linear Medium Density Polyethylene (LMDPE), Film
This property data is a summary of similar materials in the MatWeb database for the category "Linear Medium Density Polyethylene (LMDPE), Film". Each property range of values reported is minimum and..