Polymer Property : Vicat Softening Point = 202 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 202 °C
396 °F
B
Plastcom SLOVAMID 6 NG1 GF 20 HLS PA6, 20% glass fibre, combined stability
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre, heat and wheather stabilized. Stabilized against hydrolisys. Good surface finisch. Scratch resistent.Packaging, tra..
Vicat Softening Point 202 °C
396 °F
B
Plastcom SLOVASTER® B1 GF 6 HML PBT, 6% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Vicat Softening Point 202 °C
396 °F
B
Plastcom SLOVASTER® B1 GF 6 PBT, 6% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 6 % glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
Vicat Softening Point 202 °C
396 °F
50°C/h 50N
Covestro Apec® DP 1-9379/7 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M..
Vicat Softening Point 202 °C
396 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East)
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
Vicat Softening Point 202 °C
396 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® 8032U PBT+PET (Europe-Africa-Middle East)
VALOX 8032U is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. Applications: appliance housings, door handles, mirror brackets.
Vicat Softening Point 202 °C
396 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® 8032UX PBT+PET
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Vicat Softening Point 202 °C
396 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® 8032UX PBT+PET (Asia Pacific)
VALOX 8032UX is a 30% glass fibre reinforced, UV stabilized PBT+PET blend with excellent surface finish. This grade is VALOX 8032U with improved weathering resistance. Applications: appliance housin..
Vicat Softening Point 202 °C
396 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® ENH4550 PBT
25% GF reinforced, Non-Brominated & Non-Chlorinated Flame Retardant, PBT resin.
Vicat Softening Point 202 °C
396 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics Valox® SHF434HR PBT
PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant.
Vicat Softening Point 202 °C
396 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Valox® SHF434HR PBT
PBT, Super High Flow, 20% glass reinforced,hydrolytically resistant.
Vicat Softening Point 202 °C
396 °F
B/50; ISO R306
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 202 °C
396 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66
Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie..
Vicat Softening Point 202 °C
396 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Asia Pacific)
Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie..
Vicat Softening Point 202 °C
396 °F
Rate B/50; ISO 306
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 (Europe-Africa-Middle East)
Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie..
Vicat Softening Point 202 °C
396 °F
Rate B/50; ASTM D1525
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East)
Conductive GTX, CTE 6
Vicat Softening Point 202 °C
396 °F
B/50; ISO R306
Samsung Cheil Industries Infino® VB-5150GL PBT, 15% Glass Filled FR
Information provided by Samsung Cheil Industries.
Vicat Softening Point 202 °C
396 °F
ISO 306
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6
TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec..
Vicat Softening Point 202 °C
396 °F
ASTM D1525
Toyobo PELPRENE™ PE450B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.
Vicat Softening Point 202 °C
396 °F
ASTM D1525
Toyobo Pelprene™ S-6001 Polyester TPE
Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block..
Vicat Softening Point 202 °C
396 °F
ASTM D1525
Toyobo PELPRENE™ S6002 Polyester TPE, Ultra Heat-resistant
Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo.
Vicat Softening Point 202 °C
396 °F
Covestro Apec® HT KU 1-9373 High-Heat Polycarbonate
Transparent and opaque shades possible, UV-stabilized.Applications: Lighting, automotive and household goods, light covers.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience..
Vicat Softening Point 202 °C
396 °F
B/120; ISO 306
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded
Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer..
Vicat Softening Point 202 °C
396 °F
B/50; ISO 306
Eurostar Starflam B28UL PA6, Flame Retardant, Injection Molded
Starflam B28UL is Unfilled Halogen Free and Red Phosphorous Free, Flame Retardant, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
Vicat Softening Point 202 °C
396 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® VX4015 PBT (Europe-Africa-Middle East)
VALOX VX4015 is a 15% glass reinforced PBT injection moulding resin, with excellent hydrolytical stability.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Vicat Softening Point 202 °C
396 °F
Rate B/120; ISO 306
SABIC Innovative Plastics Valox® VX4510 PBT (Europe-Africa-Middle East)
VALOX VX4510 is a flame retarded, 10% glassfiber reinforced injection moulding PBT resin.