Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 58.3 - 119 °C | 137 - 246 °F | Average value: 100 °C Grade Count:231 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Vicat Softening Point | 58.3 °C | 137 °F | 50°C/hr; 50N; ASTM D1525 |
Arkema Group Solarkote® P-610 Acrylic PVC Capstock, clear, low glossInformation provided by Arkema Group |
|||
Vicat Softening Point | 58.3 °C | 137 °F | 50°C/hr; 50N; ASTM D1525 |
Arkema Group Solarkote® P-600 Acrylic PVC Capstock, clear, high glossInformation provided by Arkema Group |
|||
Vicat Softening Point | 58.3 °C | 137 °F | 50°C/hr; 50N; ASTM D1525 |
Arkema Group Solarkote® P-601 Acrylic PVC Capstock, white, high glossInformation provided by Arkema Group |
|||
Vicat Softening Point | 58.3 °C | 137 °F | 50°C/hr; 50N; ASTM D1525 |
Arkema Group Solarkote® P-611 Acrylic PVC capstock, white, low glossInformation provided by Arkema Group |