Arkema Group Solarkote® P-601 Acrylic

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, General Purpose, Molded
Manufacturer Arkema
Trade Name SolarKote®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Solarkote® P-601 Acrylic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PVC Capstock, white, high glossInformation provided by Arkema Group
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Water Absorption 0.40 %
0.40 %
weight gain after 24 hr. immersion; ASTM D570
Melt Flow 1.1 g/10 min

@Load 3.80 kg,
Temperature 230 °C
1.1 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 69
69
ASTM D785
Tensile Strength, Ultimate 20.7 MPa
3000 psi
ASTM D638
Elongation at Break 85 %
85 %
ASTM D638
Tensile Modulus 1.34 GPa
194 ksi
ASTM D638
Flexural Strength <= 33.1 MPa
<= 4800 psi
ASTM D790
Flexural Modulus 1.17 GPa
170 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm
1.60 ft-lb/in
ASTM D256
Taber Abrasion, mg/1000 Cycles 16.5
16.5
500 g load; ASTM D1044
Thermal Properties Metric English Comments
CTE, linear 117 µm/m-°C

@Temperature -17.8 °C
65.0 µin/in-°F

@Temperature 0.000 °F
ASTM E831
124 µm/m-°C

@Temperature -6.67 °C
69.0 µin/in-°F

@Temperature 20.0 °F
ASTM E831
137 µm/m-°C

@Temperature 23.9 °C
76.0 µin/in-°F

@Temperature 75.0 °F
ASTM E831
149 µm/m-°C

@Temperature 37.8 °C
83.0 µin/in-°F

@Temperature 100 °F
ASTM E831
Thermal Conductivity 0.216 W/m-K
1.50 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 51.7 °C
125 °F
annealed; ASTM D648
Vicat Softening Point 58.3 °C
137 °F
50°C/hr; 50N; ASTM D1525
68.9 °C
156 °F
50°C/hr; 10N; ASTM D1525