Thermal Properties Metric English Comments
Vicat Softening Point 38.3 - 92.2 °C
101 - 198 °F
Average value: 68.0 °C Grade Count:39
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Vicat Softening Point 38.3 °C
101 °F
ASTM D1525
ExxonMobil ESCOR™ AT 325 Molding, extrusion and compounding resin  (discontinued **)
ESCOR AT 325 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials. It has the highest melt index and the lowest modulus of all the Escor Acid Terpoly..
Vicat Softening Point 38.3 °C
101 °F
ASTM D1525
ExxonMobil Escorene™ UL 7511 Ethylene Vinyl Acetate Copolymer
Product Description: Escorene Ultra UL 7511 is a very high flow, 18.5% VA copolymer that has very good compatibility with hydrocarbon tackifiers and most waxes. It is suitable for making hot melt ad..
Vicat Softening Point 38.3 °C
101 °F
ASTM D1525
Americas Styrenics STYRON® 484 High Impact Polystyrene
Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliances/RefrigerationPackaging/disposablesHousewaresInformation pr..