Polymer Property : Vicat Softening Point = 198 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 38.3 - 92.2 °C
101 - 198 °F
Average value: 68.0 °C Grade Count:39
Overview of materials for Ethylene Acrylic Acid
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Acrylic Acid". Each property range of values reported is minimum and maximum values of appropri..
Vicat Softening Point 80.0 - 92.0 °C
176 - 198 °F
Average value: 86.3 °C Grade Count:4
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..