Material Notes:
Product CharacteristicsToughnessHeat resistanceGood stiffnessFood Contact CompliantUL Classification 94HBTypical ApplicationsLidsAppliances/RefrigerationPackaging/disposablesHousewaresInformation provided by AmericasStyrenics LLC.
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
ASTM D955
Melt Flow 2.8 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.8 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength at Break 25.5 MPa
3700 psi
ASTM D638
Tensile Strength 26.9 MPa
3900 psi
ASTM D638
Elongation at Break 65 %
65 %
ASTM D638
Tensile Modulus 1.86 GPa
270 ksi
ASTM D638
Flexural Strength 35.9 MPa
5200 psi
ASTM D790
Flexural Modulus 1.90 GPa
275 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
compression molded; ASTM D256
1.12 J/cm
2.10 ft-lb/in
injection molded; ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 31.7 °C
89.0 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 26.1 °C
79.0 °F
ASTM D648
Vicat Softening Point 38.3 °C
101 °F
ASTM D1525