Polymer Property : Shear Strength = 72.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 72.0 MPa

@Temperature 24.0 °C
10400 psi

@Temperature 75.2 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, F3T584 Carbon Fabric
Hexcel designation: F3T584-42"-F263; Fiber: T300 CelionInformation provided by HexCel
Shear Strength 72.0 MPa

@Temperature 132 °C
10400 psi

@Temperature 270 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape
Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel
Shear Strength 72.0 MPa

@Temperature -54.0 °C
10400 psi

@Temperature -65.2 °F
Short Beam
Hexcel® HexPly® F263 Epoxy Resin, W3T282 Carbon Fabric
Hexcel designation: W3T282-42"-F263; Fiber: T300 CelionInformation provided by HexCel
Shear Strength 72.0 MPa

@Temperature 177 °C
10400 psi

@Temperature 351 °F
IM7 (12K); [+/- 45°]2s; In Plane; Wet condition
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form
Fiber: IM7-12KInformation provided by HexCel