Polymer Property : Shear Strength = 4609.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 31.778 MPa

@Temperature 24.0 °C
4609.0 psi

@Temperature 75.2 °F
Lap shear
Hexcel® HexPly® F185 Epoxy Resin, 1581 Glass Fabric
Hexcel designation: 1581-38"-F185; Fiber: 150-1/2Information provided by HexCel