Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 31.778 MPa @Temperature 24.0 °C |
4609.0 psi @Temperature 75.2 °F |
Lap shear |
Hexcel® HexPly® F185 Epoxy Resin, 1581 Glass Fabric Hexcel designation: 1581-38"-F185; Fiber: 150-1/2Information provided by HexCel |