Mechanical Properties Metric English Comments
Shear Strength 11.7 MPa

@Temperature 93.3 °C
1700 psi

@Temperature 200 °F
ASTM D732
Greene Tweed Avalon® 56 PTFE
PTFE is used in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use..
Shear Strength 11.7 MPa

@Temperature 93.3 °C
1700 psi

@Temperature 200 °F
Lap Shear
Hexcel® Redux® 335M Adhesive film for bonding metallic and composite components (0.06 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..
Shear Strength 11.7 MPa

@Temperature 121 °C
1700 psi

@Temperature 250 °F
Aluminum Overlap
3M Scotch-Weld™ 2214 Hi-Dense Epoxy Adhesive
3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% ..
Shear Strength 11.7 MPa

@Temperature 23.0 °C
1700 psi

@Temperature 73.4 °F
Overlap, FRP, Substrate Failure
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive
3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as ..
Shear Strength 11.7 - 12.1 MPa

@Temperature 23.0 °C
1700 - 1750 psi

@Temperature 73.4 °F
Overlap Copper/Copper (MEK Wiped); ASTM D1002-72
3M Scotch-Weld™ DP270 Black Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M
Shear Strength 11.7 - 12.1 MPa

@Temperature 23.0 °C
1700 - 1750 psi

@Temperature 73.4 °F
Overlap Copper/Copper (MEK Wiped); ASTM D1002-72
3M Scotch-Weld™ DP270 Clear Structural Adhesive
Rigid potting compound, Non-corrosiveInformation provided by 3M