Greene Tweed Avalon® 56 PTFE

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Molded
Manufacturer Greene Tweed
Trade Name Avalon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Greene Tweed Avalon® 56 PTFE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE is used in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use in almost any applications. PTFE is visco-elastic, providing a functional seal when other fluorinated plastics such as PFA or FEP cannot. However, because virgin PTFE will creep under load its ability to provide a reliable seal during temperature cycling is limited.Ferrule gaskets made from Avalon® 56 provide a level of performance superior to other PTFE materials used in the pharmaceutical and hygienic fluid handling industries. Greene Tweed’s Avalon 56 uses the latest generation modified PTFE. Modified PTFE contains a small amount of a perfluoroether to improve creep resistance, compressive strength and permeation resistance. Modified PTFE is not only the material of choice for PTFE-faced diaphragm materials, but it is also FDA compliant.While other gasket manufacturers fabricate gaskets by directly molding the finished part, Greene Tweed machines Avalon 56 sanitary gaskets and custom shapes from isostatic-molded billets to provide optimal physical properties and tighter tolerances, easing the installation process.Avalon 56 virgin PTFE seals deliver improved sealing performance over standard PTFE.Avalon 56 is available in all sanitary gasket sizes, as well as custom shapes.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.18 g/cc
2.18 g/cc
ASTM D792
Deformation 3.2 %
3.2 %
2000 psi 78°F; ASTM D621
Mechanical Properties Metric English Comments
Tensile Strength, Yield 34.5 MPa
5000 psi
ASTM D1457
Elongation at Break 450 %
450 %
ASTM D1457
Shear Strength 9.31 MPa

@Temperature 204 °C
1350 psi

@Temperature 400 °F
ASTM D732
10.3 MPa

@Temperature 149 °C
1500 psi

@Temperature 300 °F
ASTM D732
11.7 MPa

@Temperature 93.3 °C
1700 psi

@Temperature 200 °F
ASTM D732
12.8 MPa

@Temperature 65.6 °C
1850 psi

@Temperature 150 °F
ASTM D732
15.2 MPa

@Temperature 37.8 °C
2200 psi

@Temperature 100 °F
ASTM D732
16.5 MPa

@Temperature 26.7 °C
2400 psi

@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Dynamic 0.080
0.080
33.3 psi @ 150 fpm
Coefficient of Friction, Static 0.050
0.050
33.3 psi
K (wear) Factor 5040 x 10-8 mm³/N-M
2500 x 10-10 in³-min/ft-lb-hr