Material Notes:
3M™ Scotch-Weld™ Adhesive 2214 Hi-Dense is a deareted version of Scotch-Weld adhesive 2214 regular for use where a very dense, void free bondline is required. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phenolicsInformation provided by 3M
Physical Properties Metric English Comments
Viscosity 60 - 200 cP
60 - 200 cP
Mechanical Properties Metric English Comments
Hardness, Shore D >= 85
>= 85
Tensile Strength, Ultimate 68.9 MPa
10000 psi
Elongation at Break <= 2.0 %
<= 2.0 %
Modulus of Elasticity 5.17 GPa
750 ksi
Shear Strength 2.76 MPa

@Temperature 177 °C
400 psi

@Temperature 351 °F
Aluminum Overlap
4.14 MPa

@Temperature 149 °C
600 psi

@Temperature 300 °F
Aluminum Overlap
11.7 MPa

@Temperature 121 °C
1700 psi

@Temperature 250 °F
Aluminum Overlap
20.7 MPa

@Temperature -53.0 °C
3000 psi

@Temperature -63.4 °F
Aluminum Overlap
31.0 MPa

@Temperature 24.0 °C
4500 psi

@Temperature 75.2 °F
Aluminum Overlap
31.0 MPa

@Temperature 82.0 °C
4500 psi

@Temperature 180 °F
Aluminum Overlap
Thermal Properties Metric English Comments
CTE, linear 49.0 µm/m-°C

@Temperature 0.000 - 80.0 °C
27.2 µin/in-°F

@Temperature 32.0 - 176 °F
Thermal Conductivity 0.399 W/m-K
2.77 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Volume Resistivity 2.80e+13 ohm-cm
2.80e+13 ohm-cm
Surface Resistance 9.80e+12 ohm
9.80e+12 ohm
Dielectric Constant 10.5

@Temperature 23.0 °C
10.5

@Temperature 73.4 °F
ASTM D150
11.1

@Temperature 60.0 °C
11.1

@Temperature 140 °F
ASTM D150
16.7

@Temperature 90.0 °C
16.7

@Temperature 194 °F
ASTM D150
24

@Temperature 104 °C
24

@Temperature 219 °F
ASTM D150
Dielectric Strength 3.03 kV/mm

@Thickness 0.930 mm
77.0 kV/in

@Thickness 0.0366 in
Dissipation Factor 0.126

@Temperature 23.0 °C
0.126

@Temperature 73.4 °F
0.346

@Temperature 90.0 °C
0.346

@Temperature 194 °F
0.463

@Temperature 60.0 °C
0.463

@Temperature 140 °F
0.515

@Temperature 104 °C
0.515

@Temperature 219 °F
Arc Resistance 76 sec
76 sec
Descriptive Properties Value Comments
Appearance Gray