Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 101 MPa @Temperature -55.0 °C |
14600 psi @Temperature -67.0 °F |
0° Short Beam, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 101 MPa @Temperature 25.0 °C |
14600 psi @Temperature 77.0 °F |
+/- 45° In-Plane, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, SGP370-8H Fiber Information provided by HexCel |
|||
Shear Strength | 101 MPa @Temperature 23.0 °C |
14600 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Shear Strength | 101 MPa @Temperature 23.0 °C |
14600 psi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |