Polymer Property : Flexural Strength = 75.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 75.0 MPa

@Temperature 275 °C
10900 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
Flexural Strength 75.0 MPa

@Temperature 275 °C
10900 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Flexural Strength 75.0 MPa

@Temperature 275 °C
10900 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Flexural Strength 75.0 MPa

@Temperature 275 °C
10900 psi

@Temperature 527 °F
ISO 178
Victrex® WG102™ Polyaryletherketone
Product Description: High performance thermoplastic material, PolyArylEtherKetone (PAEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact compliantWG102 does not c..
Flexural Strength 75.0 MPa

@Strain 8.00 %
10900 psi

@Strain 8.00 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 75.0 MPa

@Strain 8.50 %
10900 psi

@Strain 8.50 %
Conditioned; ISO 178
Lanxess Durethan® BKV 215 H3.0 000000 Nylon 6-Copolymer, 15% Glass Fibers
PA 6-Copolymer, 15% glass fibers, injection molding, impact modified
Flexural Strength 75.0 MPa

@Strain 6.90 %
10900 psi

@Strain 6.90 %
cond., 2 mm/min; ISO 178-A
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber
PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS.
Flexural Strength 75.0 MPa

@Temperature 80.0 °C
10900 psi

@Temperature 176 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 75.0 MPa

@Temperature 23.0 °C
10900 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.0%); ASTM-D790
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 75.0 MPa

@Temperature 23.0 °C
10900 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 75.0 MPa

@Temperature 175 °C
10900 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..