Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 441 MPa @Temperature 21.1 °C |
64000 psi @Temperature 70.0 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Strength | 441 MPa @Thickness 1.57 mm |
64000 psi @Thickness 0.0620 in |
LW |
Industrial Laminates/Norplex MC514MG Glass Fabric Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo.. |