Polymer Property : Flexural Strength = 441 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 441 MPa

@Temperature 21.1 °C
64000 psi

@Temperature 70.0 °F
Wet; ASTM D790
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 285 Kevlar® Reinforced
Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle..
Flexural Strength 441 MPa

@Thickness 1.57 mm
64000 psi

@Thickness 0.0620 in
LW
Industrial Laminates/Norplex MC514MG Glass Fabric
Description: MC514MG is made with a woven glass fabric in combination with high temperature, conductive, phenolic resin system.NP514MG has excellent flexural, compressive and impact strengths at roo..