Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 205 MPa

@Strain 4.30 %
29700 psi

@Strain 4.30 %
ISO 178
Lanxess Durethan® BKV 230 H3.0 000000 Nylon 6-Copolymer, 30% Glass Fibers
PA 6-Copolymer, 30% glass fibers, injection molding, impact modified, heat-ageing stabilized
Flexural Strength 205 MPa

@Strain 6.00 %
29700 psi

@Strain 6.00 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber
PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS.
Flexural Strength 205 MPa

@Strain 5.30 %
29700 psi

@Strain 5.30 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 15 DUS008 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 15% glass fibers, injection moldingInformation provided by LANXESS.
Flexural Strength 205 MPa

@Temperature 100 °C
29700 psi

@Temperature 212 °F
4; ISO 178
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry)
Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica..
Flexural Strength 205 MPa

@Temperature 23.0 °C
29700 psi

@Temperature 73.4 °F
DAM; ASTM D790
DuPont Performance Polymers Zytel® 80G33HS1L BK104 Nylon 66  (Unverified Data**)
Zytel® 80G33HS1L BK104 is a 33% glass fiber reinforced, heat stabilized black polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Information provide..