Mechanical Properties Metric English Comments
Flexural Strength 190 MPa

@Temperature 125 °C
27600 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 150GL20 Polyetheretherketone, 20% Glass Fibre Reinforced
Product Description:High performance thermoplastic material, 20% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Flexural Strength 190 MPa

@Temperature 125 °C
27600 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F..
Flexural Strength 190 MPa

@Temperature 125 °C
27600 psi

@Temperature 257 °F
Result based on 450GL30; ISO 178
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Flexural Strength 190 MPa

@Temperature 175 °C
27600 psi

@Temperature 347 °F
ISO 178
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
Flexural Strength 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
ISO 178
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, ..
Flexural Strength 190 MPa

@Temperature 1000 °C
27600 psi

@Temperature 1830 °F
McDanel Advanced Ceramics MV-HR1 Mullite
Mullite (3Al2O3 • 2SiO2) is a refractory oxide material combining low thermal expansion, good mechanical strength, and resilience at elevated temperatures. Mullite is formulated to produce den..
Flexural Strength 190 MPa

@Strain 2.70 %
27600 psi

@Strain 2.70 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® DP AKV 30 FN00 DUS013 Nylon 66, 30% Glass Fiber
PA 66, 30% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
Flexural Strength 190 MPa

@Temperature 23.0 °C
27600 psi

@Temperature 73.4 °F
Practical Use; ASTM-D790
Toyobo GLAMIDE® T-669VGB Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 190 MPa

@Treatment Temp. 50.0 °C,
Time 3600 sec
27600 psi

@Treatment Temp. 122 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Flexural Strength 190 MPa

@Thickness >=100 mm
27600 psi

@Thickness >=3.94 in
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM H Polyester, Glass Mat, Creme, Sheets
Description: A reasonably-priced alternative to other high-temperature types. Low thermal conductivity. Applications: Used as, among other things, thermal insulation plates where high strength prope..
Copyright © lookpolymers.com All Rights Reserved