Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 12.0 MPa @Temperature 275 °C |
1740 psi @Temperature 527 °F |
Result based on 450G; ISO 178 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Flexural Strength | 12.0 MPa @Strain 9.00 % |
1740 psi @Strain 9.00 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® BC 700 HTS DUSXBL 900116 Nylon 6, Impact Modified PA 6, non-reinforced, blow molding, impact modified, heat-aging stabilizedInformation provided by LANXESS. |
|||
Flexural Strength | 12.0 MPa @Strain 9.00 % |
1740 psi @Strain 9.00 % |
Conditioned; ISO 178 |
Lanxess Durethan® BC 700 HTS 900116 Nylon 6/66
(discontinued **) PA 6/66 |