Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 135 MPa

@Strain 5.50 %
19600 psi

@Strain 5.50 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 215 H2.0 DUS008 901510 Nylon 6, Impact Modified
PA 6, 15% glass fibers, injection molding, impact modified, heat-aging stabilizedInformation provided by LANXESS.
Flexural Strength 135 MPa

@Strain 5.80 %
19600 psi

@Strain 5.80 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® DP A 30 S FN30 DUS025 000000 Nylon 66
PA 66, non-reinforced, injection molding, halogen free flame retardant improved flowabilityInformation provided by LANXESS.
Flexural Strength 135 MPa

@Temperature 23.0 °C
19600 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 2.4%); ASTM-D790
Toyobo GLAMIDE® T-714E Transparent Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 135 MPa

@Temperature 80.0 °C
19600 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-791HT 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 135 MPa

@Temperature 250 °C
19600 psi

@Temperature 482 °F
ISO 178
Vyncolit Neopreg Kinel® SK4525 S5 Glass Fiber Reinforced Molding Compound
BMI molding compound long glass fiber reinforced with excellent mechanical and thermal properties. Especially suited to be used for injection molding.Information provided by Sumitomo Bak North Ameri..