Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 10.9 kN/m | 62.0 pli | Side 1; ASTM D624 |
Arlon 18646B026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi.. |
|||
Tear Strength | 10.9 kN/m | 62.0 pli | Side 1 Silicone Property; ASTM D624 |
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene |