Polymer Property : Tear Strength = 10.9 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 10.9 kN/m
62.0 pli
Side 1; ASTM D624
Arlon 18646B026 0.026" (0.66 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: 11523 Style FiberglassSide 2: Uncured Silicone RubberInterleave: PolyethyleneThis data represents typical values for the production materi..
Tear Strength 10.9 kN/m
62.0 pli
Side 1 Silicone Property; ASTM D624
Arlon 19646B025 Silicone Rubber/Fiberglass Laminate
Side 1:cured silicone rubber; Substrate: 1523 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil Polyethylene