Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.20 kN/m | 6.85 pli | BS EN ISO 8067 1995 |
Zotefoams Plastazote® LD45FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Tear Strength | 1.20 kN/m | 6.85 pli | Die C; ASTM D624 |
Covestro Bayfill® 380 Polyurethane Semi-Rigid Foam, Polymeric Catalyst, Open Pour, MDI-based 2-Component Liquid System Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |