Mechanical Properties Metric English Comments
Tear Strength 31.0 - 48.0 kN/m
177 - 274 pli
ASTM D 624
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..