Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 31.0 - 48.0 kN/m | 177 - 274 pli | ASTM D 624 |
API Megol AM SV/P SEBS Adhesion Modified Overmolding for Polar Polymers Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as .. |