Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tear Strength = 32.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 32.0 kN/m
183 pli
D624
Polykemi AB POLYelast TPE Z706 Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
Tear Strength 32.0 kN/m
183 pli
D624
Polykemi AB POLYelast TPE Z706EX Thermoplastic Elastomer, SEBS-based
Information provided by Polykemi AB
Tear Strength 32.0 kN/m
183 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 32.0 kN/m
183 pli
Die B
Momentive Performance Materials Siloprenâ„¢ FSL 7661 Fluorinated Liquid Silicone Rubber
This LSR elastomer is a fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperature..
Tear Strength 32.0 kN/m
183 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LIM 6041 Liquid Silicone Rubber - Healthcare Radio Opaque (X-Ray Detectability)
LSR elastomers are a two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated temperatures. The molding ..
Tear Strength 32.0 - 44.0 kN/m
183 - 251 pli
NF EN ISO 1421
Isoflon Tisoflon® 14S Silicone Coated Glass Fabric
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
Tear Strength 32.0 kN/m
183 pli
Shin-Etsu Silicones LIMSâ„¢ KEG2000-40A/B Elastomer
KEG2000-40 is a fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to..
Tear Strength 32.0 kN/m
183 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3160 Thermoplastic Elastomer
A low hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3160 can be processed by injection molding or extrusion for ap..
Tear Strength 32.0 kN/m
183 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3460 Thermoplastic Elastomer
A NSF certified, low hardness and multi-purpose thermoplastic elastomer (black and natural color) featuring excellent fluid resistance and high temperature performance. It can be processed by inject..
Tear Strength 32.0 kN/m
183 pli
ASTM D2240
UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Tear Strength 32.0 kN/m
183 pli
Trelleborg R320 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 32.0 kN/m
183 pli
Die C
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR Zinc Stearate
MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst..
Tear Strength 32.0 kN/m
183 pli
ASTM D624
ELASTO UK Dryflex® 400701S SBS Based Material, 70A Hardness, Natural
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
Tear Strength 32.0 kN/m
183 pli
ASTM D624
ELASTO UK Dryflex® 402701S SBS Based Material, 70A Hardness, Black
The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for..
Tear Strength 32.0 kN/m
183 pli
ASTM D624
ELASTO UK Dryflex® 500700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Tear Strength 32.0 kN/m
183 pli
ASTM D624
ELASTO UK Dryflex® 502700S SEBS Based Material, Unfilled Qualities, 70A Hardness, Black
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Tear Strength 32.0 kN/m
183 pli
ASTM D624
ELASTO UK Dryflex® 600700S SEBS Based Material, Filled Qualities, 70A Hardness, Natural
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
Tear Strength 32.0 kN/m
183 pli
ASTM D624
ELASTO UK Dryflex® 602700S SEBS Based Material, Filled Qualities, 70A Hardness, Black
The most significant features of the 600-series are the improved heat stability, the sound reduction and that the material enables an easy and secure pigmenting for the customer. A filled material ..
Tear Strength 32.0 kN/m
183 pli
ISO 34-B
AlphaGary Evoprene™ 022 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Tear Strength 32.0 kN/m
183 pli
Die C; Cross direction; ASTM D624
Teknor Apex Sarlink® 3460N Thermoplastic Elastomer
A NSF certified, colorable, multi-purpose thermoplastic elastomer featuring excellent fluid resistance and high temperature performance. It can be processed by injection molding, blow molding or ext..
Copyright © lookpolymers.com All Rights Reserved