Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR130B Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
ASTM D412
Tensile Strength at Break 14.8 MPa
2150 psi
ASTM D412
Elongation at Break 470 %
470 %
ASTM D412
100% Modulus 0.00180 GPa
0.261 ksi
ASTM D412
200% Modulus 0.00430 GPa
0.624 ksi
ASTM D412
300% Modulus 0.00760 GPa
1.10 ksi
ASTM D412
Tear Strength 32.0 kN/m
183 pli
ASTM D2240
Users viewing this material also viewed the following: