Isoflon Tisoflon® 14S Silicone Coated Glass Fabric

Category Ceramic , Glass , Glass Fiber , Polymer , Thermoset , Silicone
Manufacturer Isoflon
Trade Name Tisoflon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Isoflon Tisoflon® 14S Silicone Coated Glass Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Silicone coated Glass fabric TISOFLON®Information provided by Isoflon.
Physical Properties Metric English Comments
Thickness 350 microns
13.8 mil
Coating Weight 490 g/m²
306 lb/ream
entire thickness; NF EN ISO 2286.2
Mechanical Properties Metric English Comments
Tear Strength 32.0 - 44.0 kN/m
183 - 251 pli
NF EN ISO 1421
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Descriptive Properties Value Comments
Color white or red
Silicone Content (%) 59