Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 40.8 kN/m | 233 pli | post cured- 4 hours at 204°C; Die B |
Multibase SILASTIC® C7-4565 VAROX Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 40.8 kN/m | 233 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90450 Polyvinyl Chloride, Flexible (PVC, Flexible) Automotive OEM approval(s).Information provided by PolyOne |
|||
Tear Strength | 40.8 kN/m | 233 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.8 kN/m | 233 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 65-HR-9 TPE Product Description: StarTUFF TF 65-HR-9 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Tear Strength | 40.8 kN/m | 233 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 3.0 PHR Thanecure ZM MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.8 kN/m | 233 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Di-Cup 40C Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
Tear Strength | 40.8 kN/m | 233 pli | ASTM D1004 |
Bayshore Vinyl Compounds BVC 7200-75 Vinyl Compound BVC 7200-75 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a s.. |
|||
Tear Strength | 40.8 kN/m | 233 pli | Die C |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 1.0 PHR Di-Cup 40C Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |