PolyOne Geon™ Vinyl Flexible 90450 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible 90450 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
15 sec; ASTM D2240
Tensile Strength at Break 11.8 MPa
1710 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 400 %
400 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 40.8 kN/m
233 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Flame Spread 0.00 mm/min
0.00 in/min
Automotive Burn Test; FMVSS 302
Descriptive Properties Value Comments
Automotive Specifications FORD WSK-M4D871-A1
Cold Flexibility Pass
GM 9503P; -29°C, 1.91 mm; 25 mm, 4 hr
Features Low Gloss
Fogging 86%
SAE J1756; 3 hrs, 212°F(100°C), 70°F(21°C), after 1 hour
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Interior Trim
Xenon Weatherometer Pass
SAE J1960; Interior, 1240 kJ/m², All Colors, dE*<3.0