Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 0.500 kN/m | >= 2.85 pli | Die C; ASTM D624 |
Rogers Corporation Poron® 4701-30-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Tear Strength | >= 0.500 kN/m | >= 2.85 pli | Die C; ASTM D624 |
Rogers Corporation Poron® 4701-40-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Tear Strength | 0.500 kN/m | 2.85 pli | |
Fujipoly Industries Sarcon® 30Q Thin-Film QR Sarcon QR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Tear Strength | 0.500 kN/m | 2.85 pli | ASTM D 624 |
Eurofoam Porocell POR 304 F-7142 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |
|||
Tear Strength | 0.500 kN/m | 2.85 pli | ASTM D 624 |
Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |