Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Eurofoam s.r.l.
Trade Name POROCELL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eurofoam Porocell POR 300/100 Ethylene Octane Metallocene EPDM Foam.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Physical Properties Metric English Comments
Density 0.0900 - 0.110 g/cc
0.00325 - 0.00397 lb/in³
ISO 845-88
Water Absorption 0.12 %
0.12 %
ASTM D 1056
Mechanical Properties Metric English Comments
Hardness, Shore OO 45 - 55
45 - 55
ASTM D 2240
Tensile Strength 0.900 MPa
131 psi
ASTM D 412
Elongation at Break >= 300 %
>= 300 %
ASTM D 412
Compressive Yield Strength 0.0500 MPa

@Strain 25.0 %
7.25 psi

@Strain 25.0 %
ASTM 1056/85
0.120 MPa

@Strain 50.0 %
17.4 psi

@Strain 50.0 %
ASTM 1056/85
Tear Strength 0.500 kN/m
2.85 pli
ASTM D 624
Compression Set 15 %

@Strain 25.0 %
15 %

@Strain 25.0 %
ASTM D 395
25 %

@Strain 50.0 %
25 %

@Strain 50.0 %
ASTM D 395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
ASTM D 3575
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
ASTM D 3575
Shrinkage <= 5.0 %

@Temperature 70.0 °C,
Time 605000 sec
<= 5.0 %

@Temperature 158 °F,
Time 168 hour
Linear; ASTM D 1204
Descriptive Properties Value Comments
Cellular Structure Closed
Color Black, White, Grey
Declaration of Heavy Metal Absence Conform
RoHS2002/95/EC
Fire Resistance MV22 302
Pass
Vulcanization Peroxide
Users viewing this material also viewed the following: