Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 18.9 kN/m | 108 pli | as molded; Die B |
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 18.9 kN/m | 108 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Tear Strength | 18.9 kN/m | 108 pli | Die B, Silicone Property; ASTM D624 |
Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured SiliconeInterleave 2: Polyethylene This data represents typical values .. |
|||
Tear Strength | 18.9 kN/m | 108 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 191-70PA Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft .. |
|||
Tear Strength | 18.9 kN/m | 108 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Geolast® 701-70 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |