Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 19.0 kN/m | 108 pli | ASTM D624-95 |
Multibase Multi-Flex® TPO D 6006 Grey Data provided by Multibase. |
|||
Tear Strength | 18.9 kN/m | 108 pli | as molded; Die B |
Multibase SILASTIC® C7-4535 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 19.0 kN/m | 108 pli | ISO 34-1 |
PolyOne OnFlex™ S EH 40A-3S7001 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tear Strength | 19.0 kN/m | 108 pli | ISO 34-1 |
PolyOne OnFlex™ S EH 50A-3S7002 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tear Strength | 19.0 kN/m | 108 pli | D624 |
Polykemi AB POLYelast TPE Z500 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
Tear Strength | 19.0 kN/m | 108 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FFSL 7061 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tear Strength | 19.0 kN/m | 108 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ FFSL 7071 Fully Fluorinated Liquid Silicone Rubber This LSR elastomer is a fully fluorinated, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempe.. |
|||
Tear Strength | 19.0 kN/m | 108 pli | |
Trelleborg E450 EPDM Rubber EPM -- EPDM or Ethylene -- Propylene Rubber. EPM can only be vulcanized by peroxides or radiation; whereas EPDM can be vulcanized conventionally using sulphur.Properties:Excellent inherent high and .. |
|||
Tear Strength | 18.9 kN/m | 108 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Santoprene® 8271-65 Thermoplastic Elastomer A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It complies with FDA regulations for rubber articles intended for repeated .. |
|||
Tear Strength | 19.0 kN/m | 108 pli | Parallel to flow; ISO 34-B |
AlphaGary Evoprene™ LF 6154 Automotive Thermoplastic Elastomer Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab.. |
|||
Tear Strength | 18.9 kN/m | 108 pli | Die B, Silicone Property; ASTM D624 |
Arlon R38081R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassSide 2: Uncured SiliconeInterleave 2: Polyethylene This data represents typical values .. |
|||
Tear Strength | 19.0 kN/m | 108 pli | |
ACC MM913 Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: high tear strength, picks up extremely fine details, low viscosity, good resistance to styrene attack, easy degassing.. |
|||
Tear Strength | 18.9 kN/m | 108 pli | 73°F, Die C; ASTM D624 |
ExxonMobil Santoprene® 191-70PA Thermoplastic Elastomer
(discontinued **) A soft, black, specialty thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. It is especially formulated to bond to PA-6 and blends thereof for applications where hard/soft .. |
|||
Tear Strength | 18.9 kN/m | 108 pli | 73°C, Die C; ASTM D624 |
ExxonMobil Geolast® 701-70 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |