PolyOne Synprene® RT-3850E Thermoplastic Elastomer - SBC  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3850E Thermoplastic Elastomer - SBC  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastomers. These materials are ideal for applications requiring flexibility over a wide temperature range, excellent colorability, broad processing capability and durability.Description/Features:High Performance Thermoplastic ElastomerNaturalApplications: Multi-PurposeFDA (Food contact)Processing Method: ExtrusionInformation provided by PolyOne Corporation
Physical Properties Metric English Comments
Specific Gravity 0.890 g/cc
0.890 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 49
49
10 Sec; ASTM D2240
52
52
Instant; ASTM D2240
Tensile Strength, Yield 5.86 MPa
850 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
3.59 MPa

@Strain 300 %
520 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 680 %
680 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 21.0 kN/m
120 pli
Die C (graves), 20 in/min; ASTM D624