Mechanical Properties Metric English Comments
Tear Strength 2.00 - 113 kN/m
11.4 - 645 pli
Average value: 24.8 kN/m Grade Count:768
Overview of materials for Styrenic Elastomer (TES)
This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro..
Tear Strength 73.5 - 113 kN/m
420 - 644 pli
Taiwan PU Corporation PPG CPU-2079 Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..
Tear Strength 73.5 - 113 kN/m
420 - 644 pli
Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu..