Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Rubber or Thermoset Elastomer (TSE)
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation PTMG CPU-100L Polyurethane Casting Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing.Information provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Viscosity 10000 - 30000 cP

@Temperature 40.0 °C
10000 - 30000 cP

@Temperature 104 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 88 - 92
88 - 92
Tensile Strength at Break 28.44 - 43.15 MPa
4125 - 6258 psi
Elongation at Break 395 - 495 %
395 - 495 %
Tear Strength 73.5 - 113 kN/m
420 - 644 pli
Processing Properties Metric English Comments
Processing Temperature 100 °C
212 °F
Working Temperature, Prepolymer
Mold Temperature 100 °C
212 °F
Pot Life 11 min
11 min
Descriptive Properties Value Comments
MOCA Temperature 110°C
NCO Content Max 4.4%
Min 4%
PHR of MOCA 12.5%
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved