Material Notes:
A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, curing, demolding and after curing.Information provided by Taiwan PU Corporation.
Physical Properties Metric English Comments
Viscosity 9000 - 14000 cP

@Temperature 40.0 °C
9000 - 14000 cP

@Temperature 104 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 78 - 82
78 - 82
Tensile Strength at Break 17.16 - 26.97 MPa
2489 - 3912 psi
Elongation at Break 510 - 660 %
510 - 660 %
Tear Strength 73.5 - 113 kN/m
420 - 644 pli
Processing Properties Metric English Comments
Processing Temperature 100 °C
212 °F
Working Temperature, Prepolymer
Mold Temperature 100 °C
212 °F
Pot Life 11 min
11 min
Descriptive Properties Value Comments
MOCA Temperature 110°C
NCO Content Max 4%
Min 3.6%
PHR of MOCA 11%