Polymer Property : Tear Strength = 1.80 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 1.80 kN/m
10.3 pli
Typical; ASTM D264-91 Die C
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft
Very soft, easily compressed for use where flexibility is a key requirement.  Standard available  thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi..
Tear Strength 1.80 kN/m
10.3 pli
Typical; ASTM D264-91 Die C
Rogers Corporation Poron® 4701-41-15 Urethane Foam, Soft, Enhanced Sealability
Soft, enhanced sealability material offering greater closed-cell content for demanding vacuum sealing applications or low closure-force requirements.  Standard available thickness range from 0.031"..
Tear Strength >= 1.80 kN/m
>= 10.3 pli
ASTM D642-91 Die C
Rogers Corporation Poron® Shock Seal™ 4790-79-20 Urethane Foam, Industrial Grade
Thickness: 0.062"- 0.188"Color: BlackInformation provided by Rogers Corporation.
Tear Strength >= 1.80 kN/m
>= 10.3 pli
ASTM D624, Die C
Rogers Corporation R/bak® SF Supported Firm Cushion Mounting Material
R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b..
Tear Strength >= 1.80 kN/m
>= 10.3 pli
ASTM D624, Die C
Rogers Corporation R/bak® U Unsupported Cushion Mounting Material
R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b..
Tear Strength >= 1.80 kN/m
>= 10.3 pli
ASTM D624, Die C
Rogers Corporation R/bak® U1A Cushion Mounting Material, Unsupported with Single-sided Acrylic Adhesive
R/bak materials are high-density, open cell, polyurethane foams used to build thickness on the cylinder, provide cushioning and absorb vibration in the Flexographic printing process. The use of R/b..
Tear Strength 1.80 kN/m
10.3 pli
80°C for 1,000 hrs; JIS-K-6252(Angle)/ASTM D 624
Fujipoly Industries Sarcon® NR-c Gap Filler Pad Non-Silicone
Sarcon NR-c consists of an Acrylate resin and some thermal conductive fillers. It is a highly conformable/ thermally conductive material in a versatile sheet form that makes reliable and complete p..
Tear Strength >= 1.80 kN/m
>= 10.3 pli
Die C; ASTM D624
Rogers Corporation Poron® 4701-50-20 Cellular Urethane Foam
Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h..