Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 0.700 kN/m | >= 3.99 pli | ASTM D264-91 Die C |
Rogers Corporation Poron® 4701-30-25 Urethane Foam, Very Soft Very soft, easily compressed for use where flexibility is a key requirement. Standard available thickness range from 0.021"Features and Benefits of PORON Products: Excellent compression set resi.. |
|||
Tear Strength | >= 0.700 kN/m | >= 3.99 pli | Die C; ASTM D624 |
Rogers Corporation Poron® 4701-30-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Tear Strength | >= 0.700 kN/m | >= 3.99 pli | ASTM D264-91 Die C |
Rogers Corporation Poron® 4790-92-15 Urethane Foam, Extra Soft, Slow Rebound Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression .. |
|||
Tear Strength | 0.700 kN/m | 3.99 pli | |
Fujipoly Industries Sarcon® 85U Thin-Film UR Sarcon UR is Fujipolys originally developed High Heat Conductive/Low Hardness Silicone Rubber. Fine, high heat conductive ceramic particles are mixed with insulative silicone rubber.Information prov.. |
|||
Tear Strength | 0.700 kN/m | 3.99 pli | BS EN ISO 8067 1995 |
Zotefoams Plastazote® MP24 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Tear Strength | 0.700 kN/m | 3.99 pli | ISO 8067 |
Zotefoams ZOTEK® F 35 PVDF Foam Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 12028 Black 1/8" (3.2 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 12032 Black 3/32" (2.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 12038 Black 3/8" (9.5 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 6035PC 12028 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 6035PC 12032 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 6035PC 12036 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 12026 Black 1/16" (1.6 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 12034 Black 1/4" (6.4 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 12036 Black 3/16" (4.8 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 6035PC 12026 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 6035PC 12030 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 6035PC 12034 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 6035PC 12038 Polyurethane Foam Tape (15 lb./ft3 (239 kg/m3) Series) 3M™ series polyurethane foam substrates with a high performance, pressure-sensitive acrylic adhesive on one side. 3M™ microcellular polyurethane foam is designed for high performance gasketing and.. |
|||
Tear Strength | 0.700 kN/m | 4.00 pli | |
3M 12030 Black 1/2" (12.7 mm) Polyurethane Foam High flexibility and conformability for secure seals and effective sound damping without crumbling or embrittlement Choice of medium or high density Low water absorption and good solvent resistance .. |