Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Rupture = 2.5611 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Rupture 0.017658 GPa

@Temperature 1500 °C,
Time 10800 sec
2.5611 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories CTC-63TD Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.017658 GPa

@Temperature 110 °C,
Time 86400 sec
2.5611 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-16H Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.017658 GPa

@Temperature 110 °C,
Time 86400 sec
2.5611 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-16H-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.017658 GPa

@Temperature 1000 °C,
Time 10800 sec
2.5611 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-16S-W2 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.017658 GPa

@Temperature 1000 °C,
Time 10800 sec
2.5611 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SFC-60 SiC Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.017658 GPa

@Temperature 110 °C,
Time 86400 sec
2.5611 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SFC-90W High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.017658 GPa

@Temperature 1500 °C,
Time 10800 sec
2.5611 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories PCT-AM-1 Monolithic Refractories for Ladle and Tundish
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Copyright © lookpolymers.com All Rights Reserved