Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 8.81 J | 6.50 ft-lb | Dow Method |
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP) AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi.. |
|||
Puncture Energy | 8.81 J | 6.50 ft-lb | Dow Method |
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design.. |