Polymer Property : Puncture Energy = 6.50 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 8.81 J
6.50 ft-lb
Dow Method
Dow AFFINITY™ PL 1880G Polyolefin Plastomer (POP)
AFFINITY™ PL 1880G is an ethylene alpha-olefin resin produced via INSITE™ Technologies. It is designed for use in a variety of packaging applications, including high-speed, form-fill-seal packagi..
Puncture Energy 8.81 J
6.50 ft-lb
Dow Method
Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin
Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HSE-7002 NT 7 is an ethylene-hexene-1 copolymer, design..