Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Puncture Energy = 45.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 45.0 - 60.0 J
33.2 - 44.3 ft-lb
Average value: 54.0 J Grade Count:5
Overview of materials for Polycarbonate, Unreinforced, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Unreinforced, Flame Retardant". Each property range of values reported is minimum and max..
Puncture Energy 45.0 - 47.0 J
33.2 - 34.7 ft-lb
Average value: 46.3 J Grade Count:8
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor..
Puncture Energy 45.0 - 45.0 J

@Temperature -30.0 - -30.0 °C
33.2 - 33.2 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 45.0 J Grade Count:1
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va..
Puncture Energy 45.0 J
33.2 ft-lb
ISO 6603-2
Lanxess Pocan® B 1305 000000 PBT
PBT, non-reinforced, injection molding
Puncture Energy 45.0 J
33.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman DuraStar DS2000 Polymer, Natural
Durastar DS2000 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. DS2000 has ver..
Puncture Energy 45.0 J
33.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman DuraStar DS2110UVI Polymer, Natural
Durastar DS2110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li..
Puncture Energy 45.0 J
33.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman DuraStar MN621 Polymer, Natural
Durastar Polymer MN621 was developed for the medical device industry and contains a mold release It processes easily and requires minimal drying time. It has superior toughness, high clarity and goo..
Puncture Energy 45.0 J
33.2 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar BR203 Copolyester
Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie..
Puncture Energy 45.0 J

@Thickness 3.20 mm
33.2 ft-lb

@Thickness 0.126 in
At Max load; ASTM D3763
Eastman Eastar DN114 Copolyester, Natural
Applications:LightingProduct Description: Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage. DN1..
Puncture Energy 45.0 J

@Temperature -40.0 °C
33.2 ft-lb

@Temperature -40.0 °F
Puncture Resistance at Max Load; ASTM D3763
Eastman Eastar EN076 Copolyester
Eastar Copolyester EN076 is recommended for the thick-walled containers that are prevalent in the cosmetics and personal care markets. This copolyester offers good processability with the benefits o..
Puncture Energy 45.0 J
33.2 ft-lb
ISO 6603-2
Covestro Makroblend® DP UT3907 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseUV-stabilizedinjection molding grade Makroblend DP UT3907* offers superior flowability, good impact strength and excellent ch..
Puncture Energy 45.0 J

@Temperature 23.0 °C
33.2 ft-lb

@Temperature 73.4 °F
ISO 6603-2
Covestro Makrolon® 6165 X Polycarbonate
Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Low..
Puncture Energy 45.0 J
33.2 ft-lb
ISO 6603-2
Covestro Makroblend® DP UT3905 Polycarbonate + PBT, Impact Grade
Developmental product(PC+PBT)-blendhigh flowimpact modifiedeasy releaseinjection molding grade Makroblend DP UT3905* offers superior flowability, good impact strength and excellent chemical resist..