Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 6.90 - 45.0 J | 5.09 - 33.2 ft-lb | Average value: 29.8 J Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Puncture Energy | 45.0 - 45.0 J @Temperature -30.0 - -30.0 °C |
33.2 - 33.2 ft-lb @Temperature -22.0 - -22.0 °F |
Average value: 45.0 J Grade Count:1 |
Overview of materials for Polycarbonate/ASA Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ASA Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |