Polymer Property : Puncture Energy = 42.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar 5445 PCTG Copolyester, Injection Molded  (discontinued **)
Eastar PCTG 5445 is an amorphous copolyester. Because of its clarity, toughness and good melt strength, Eastar PCTG Copolyester 5445 is useful in a number of applications. It has high gloss and is t..
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman DuraStar DS1000 Polymer, Natural
Durastar DS1000 polymer has excellent appearance and clarity. Its most outstanding features are chemical resistance and excellent processing characteristics. Exposure to aromatic oils often causes c..
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman DuraStar DS1110UVI Polymer, Natural
Durastar DS1110UVI polymer, contains an ultraviolet light stabilization package. It is recommended for indoor applications requiring enhanced color stability upon extended exposure to fluorescent li..
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman DuraStar MN610 Polymer, Natural
Durastar MN610 polymer has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing characteristics. MN610 has very ..
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman DuraStar MN611 Polymer, Natural
Durastar Polymer MN611 contains a mold release. It has excellent appearance and is nearly water-clear. Its most outstanding features are toughness, chemical resistance, and excellent processing char..
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar AN001 Copolyester, Natural
Eastar AN001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca..
Puncture Energy 42.0 J
31.0 ft-lb
Puncture Resistance @Max Load, 23°C; ASTM D3763
Eastman Eastar BR001 Copolyester
Eastar BR001 Copolyester has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilities. Exposure to aromatic oils often ca..