Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Puncture Energy | 4.90 J | 3.61 ft-lb | ISO 6603-2 |
Lanxess Durethan® BKV 315 Z H2.0 901510 Nylon 6, 15% Glass Fiber PA 6 extrusion- and blow molding-grade with 15% glass fibers, branched/structural viscosity, elastomer-modified, good heat-ageing resistance, dry-impact modifiedApplication Examples: air intake hose.. |